Questions and CORRECT Answers
Who is responsible for identifying the assembly class? - CORRECT ANSWER - User
What is a defect? - CORRECT ANSWER - A condition that may affect the form, fit, or
function of the item in the end use environment
Hardware found to not conform to the requirements of the standard shall be classified as defects
and dispositioned for: - CORRECT ANSWER - [D1D2D3]
There shall be no broken strands for wires used at a potential of 6kV or greater: - CORRECT
ANSWER - [D1D2D3]
A documented process control system shall be implemented for: - CORRECT ANSWER -
[N1N2D3]
The contract shall take precedence over this standard for: - CORRECT ANSWER -
[D1D2D3]
What is wire overlap? - CORRECT ANSWER - When a wire is wrapped more than 360
and crosses over itself
What is wire over wrap? - CORRECT ANSWER - When a wire is wrapped more than 360
and remains in contact with the terminal
Manufacturers shall perform 100% inspection unless sampling inspection is defined for: -
CORRECT ANSWER - [N1D2D3]
, Inspection of soldering and cleanliness shall be performed prior to conformal coasting, staking,
or encapsulation for: - CORRECT ANSWER - [N1D2D3]
Illumination at the surface of work stations should be at least what? - CORRECT
ANSWER - 1000 lux
What is the tolerance for magnification aids? - CORRECT ANSWER - +- 15%
Eating, drinking, smoking, e-cigs use shall be prohibited at the work station for: - CORRECT
ANSWER - [D1D2D3]
Manufacturer shall verify ESD is adequate when humidity falls below 30% for: - CORRECT
ANSWER - [N1D2D3]
Manufacturer shall establish an ESD control program for: - CORRECT ANSWER -
[D1D2D3]
What is J-STD-002? - CORRECT ANSWER - Solder-ability tests for Component leads,
terminations, lugs, wires, and terminals
What is J-STD-003? - CORRECT ANSWER - Solder ability tests for printed boards
What is J-STD-004? - CORRECT ANSWER - Requirements for Soldering Fluxes
What is J-STD-005? - CORRECT ANSWER - Requirements for Soldering Paste
What is J-STD-006? - CORRECT ANSWER - Requirements for electronic grade solder
alloys, fluxed and non-fluxed solid solders