Which of the following is the standard specification for loadbearing concrete masonry units? - ANSWERASTM C 90; RCMCI 6th Edition, Section 2.2.1 Which of the following grout admixtures is used to obtain a high slump with reduced water? - ANSWERSuper plasticizer; RCMCI 6th Edition, Section 2.11.6

Content preview

ICC MASONRY EXAM QUESTIONS &
ANSWERS
Which of the following is the standard specification for loadbearing
concrete masonry units? - ANSWERASTM C 90; RCMCI 6th Edition, Section 2.2.1

Which of the following grout admixtures is used to obtain a high
slump with reduced water? - ANSWERSuper plasticizer; RCMCI 6th Edition, Section
2.11.6

Which of the following is the standard specification that autoclaved aerated concrete
masonry units must conform to for the strength class specified in the contract
documents? - ANSWERASTM C 1386; CI 530; Part 2, Section 2.3E. IBC
2103.3

Grout intended for use in the construction of engineered and
empirically designed masonry structures must comply with - ANSWERASTM C 476;
2006 IBC 2103.12

The slump test for grout must be performed in accordance with - ANSWERASTM C
1019; ASTM - C1019-03

In what condition are grout specimens to be tested? - ANSWERDamp; ASTM - 1019-03

When the prism test method is being utilized, how long must the
prisms cure prior to being cut? - ANSWER28; 2006 IBC 2105.3.1

After construction and grouting, masonry test prisms should not be
disturbed or moved for a minimum of - ANSWER48 hours; ASTM - C 1314, Section
5.10

When field sampling grout, the elapsed time between obtaining the
first and final portions of the sample shall not be more than - ANSWER15 minutes;
ASTM - C1019, Section 7.2.1

If mortar compression tests are required, how many tests per day are to be taken for the
three successive work days at the start of the job? - ANSWER1; RCMCI 6th Edition,
3.2.4

Glass unit masonry shall not be laid at temperatures below - ANSWER60 degrees F;
2006 IBC 2104.3.2.1

, What is the maximum mean daily temperature permitted before newly constructed
masonry must be fog sprayed during curing? - ANSWER100 degrees F; 2006 IBC
2104.4.3

When the temperature is below 40 degrees F, newly constructed
masonry must be covered with a weather resistant membrane for a
minimum of - ANSWER24 hours; 2006 IBC 2104.3.3.3

After initial mixing, when the ambient temperature exceeds 90
degrees F with a wind velocity over 8 mph, mortar used in masonry
construction must be discarded after - ANSWER2 hours; 2006 IBC 2104.4.2.1

Which type of unit masonry is required to be placed with head and bed joints solidly
filled? - ANSWERGlass; 2006 IBC 2104.1.2.4

Thin bed mortar joints used in laying autoclaved aerated concrete
masonry units shall not exceed a thickness of - ANSWER1/16"; 2006 IBC 2104.1.2.6

When the ambient temperature exceeds 100 degrees F or exceeds 90 degrees F with a
wind velocity over 8 mph, what is the maximum
distance that mortar may be spread ahead of AAC masonry units? - ANSWER4';
RCMCI 6th Edition, Section 11.2.4,
2006 IBC 2104.4.2.1(5).

What is the maximum spacing for weep holes placed in the outside
wythe of masonry walls? - ANSWER33" on center; 2006 IBC 2104.1.8

The maximum corbeled projection beyond the face of the wall for
multiwythe walls bonded by mortar or grout, and wall ties or masonry
headers is - ANSWER1/2 the wall thickness; 2006 IBC 2104.2

The maximum spacing of movement joints is - ANSWER25' or three times the wall
height; ACI 530

In masonry construction, what type of joint is used to allow
dimensional changes in masonry, minimize random wall cracks and
other distress? - ANSWERMovement joint; ACI 530

In masonry construction, what is the maximum tolerance permitted
for vertical alignment of nonbearing columns and walls? - ANSWER+/- 3/4"; ACI 530, S-
21, Section 3.3G (2) (d)

Which type of mortar is used for placing adhered masonry veneer? - ANSWERType S;
ACI 530, S-2O, Section 3.3C (2)

What is the minimum thickness required for parapet walls of

Document information

Uploaded on
August 28, 2026
Number of pages
7
Written in
2026/2027
Type
Exam (elaborations)
Contains
Questions & answers
$13.99

Wrong document? Swap it for free Within 14 days of purchase and before downloading, you can choose a different document. You can simply spend the amount again.
Written by students who passed
Immediately available after payment
Read online or as PDF

Seller avatar
Reputation scores are based on the amount of documents a seller has sold for a fee and the reviews they have received for those documents. There are three levels: Bronze, Silver and Gold. The better the reputation, the more your can rely on the quality of the sellers work.
shantelleG
4.0
(118)
Sold
651
Followers
369
Items
18358
Last sold
5 days ago



Why students choose Stuvia

Created by fellow students, verified by reviews

Quality you can trust: written by students who passed their tests and reviewed by others who've used these notes.

Didn't get what you expected? Choose another document

No worries! You can instantly pick a different document that better fits what you're looking for.

Pay as you like, start learning right away

No subscription, no commitments. Pay the way you're used to via credit card and download your PDF document instantly.

Student with book image

“Bought, downloaded, and aced it. It really can be that simple.”

Alisha Student

Working on your references?

Create accurate citations in APA, MLA and Harvard with our free citation generator.

Working on your references?

Frequently asked questions