1. During a qualification test for a groove weld, the welder observes that the
root opening is smaller than specified on the qualified welding procedure
specification (WPS). What is the most appropriate action?
A. Increase amperage substantially to compensate
B. Increase travel speed to prevent burn-through
C. Stop and have the joint corrected to conform to the WPS before welding
D. Continue because root opening does not affect qualification
Answer: C. Stop and have the joint corrected to conform to the WPS before
welding
Rationale: The qualification test must be performed within the applicable
essential variables. A substantially incorrect root opening can alter penetration,
fusion, bead geometry, and the validity of the qualification.
,2. What welding discontinuity is most directly associated with failure to
properly fuse the sidewall of a groove?
A. Crater crack
B. Porosity
C. Incomplete fusion
D. Excessive reinforcement
Answer: C. Incomplete fusion
Rationale: Incomplete fusion occurs when deposited weld metal does not
properly fuse with the base metal or previously deposited weld metal. Sidewall
fusion is particularly important in groove-weld qualification.
3. In SMAW, which electrode classification is generally associated with a low-
hydrogen coating?
A. E6010
B. E6011
C. E6013
D. E7018
Answer: D. E7018
Rationale: E7018 is a low-hydrogen electrode when properly stored and
handled. Moisture control is critical because hydrogen can contribute to
hydrogen-assisted cracking.
4. Why are low-hydrogen electrodes commonly controlled carefully during
structural welding?
A. To increase arc voltage
B. To eliminate all slag
C. To reduce the potential for hydrogen-assisted cracking
D. To increase weld metal hardness in every application
Answer: C. To reduce the potential for hydrogen-assisted cracking
,Rationale: Diffusible hydrogen, combined with susceptible microstructures and
tensile stress, can contribute to hydrogen-assisted cracking. Proper electrode
storage and handling reduce the hydrogen source.
5. A welder increases welding current substantially while maintaining the same
travel speed. What is the most likely effect?
A. Reduced heat input
B. Reduced penetration
C. Increased penetration and deposition rate
D. Elimination of distortion
Answer: C. Increased penetration and deposition rate
Rationale: Increasing current generally increases arc energy and deposition rate.
Excessive current can, however, cause undercut, excessive penetration, spatter,
or other problems.
6. Which discontinuity consists of a groove melted into the base metal adjacent
to the weld toe and left unfilled?
A. Overlap
B. Undercut
C. Incomplete penetration
D. Porosity
Answer: B. Undercut
Rationale: Undercut is a reduction in base-metal thickness at the weld toe or
root caused by melting that is not subsequently filled with weld metal.
7. What is the principal purpose of preheating carbon steel before welding
when required by the applicable procedure?
A. Increase electrical conductivity
B. Eliminate all residual stress
C. Control cooling rate and reduce the risk of cracking
D. Make the weld metal nonmagnetic
, Answer: C. Control cooling rate and reduce the risk of cracking
Rationale: Preheat slows cooling, helps control the heat-affected zone
microstructure, reduces thermal gradients, and can reduce hydrogen-assisted
cracking susceptibility.
8. What is the primary function of shielding gas in GMAW?
A. Increase electrode diameter
B. Cool the base metal
C. Protect the molten weld pool from atmospheric contamination
D. Remove all slag
Answer: C. Protect the molten weld pool from atmospheric contamination
Rationale: Shielding gas prevents oxygen, nitrogen, and other atmospheric
constituents from contaminating the molten weld pool and degrading weld
quality.
9. Excessive electrode travel speed in SMAW can contribute to which condition?
A. Excessive reinforcement only
B. Insufficient fusion or inadequate bead size
C. Excessive preheat
D. Increased electrode moisture
Answer: B. Insufficient fusion or inadequate bead size
Rationale: Excessive travel speed reduces the amount of heat delivered per unit
length and can prevent adequate fusion or produce an undersized weld.
10. What is the principal reason for removing slag between SMAW passes?
A. Increase electrode moisture
B. Prevent slag inclusions and permit sound fusion of subsequent passes
C. Reduce shielding gas flow
D. Increase arc length