2026/2027 WITH 135 QUESTIONS
AND EXPERT-VERIFIED
CORRECT ANSWERS | ALREADY
GRADED A+ | GUARANTEED PASS
| NICET PRACTICE EXAM
What is the Min and Max of Dowel overlapping - ANSWER-2" to 6" and 2" of
clear cover
How are Tiebars placed and what is the spacing? - ANSWER-Drilled into the Slap
or placed in the keyway and 1' Spacing
What is the load transfer assemblies spacing - ANSWER-Every 15' 1/2"
What should be placed on forms before concrete placement? - ANSWER-Form oil
to provide neat edges
What is the Transverse joint spacing? - ANSWER-Every 4'
, When does Concrete pavement curing process begin? - ANSWER-Immediately
after finishing
How long does concrete pavement take to cure? - ANSWER-Minimum of 14 days
to achieve compressive strength
What are concrete paving curing methods - ANSWER-Burlap (Wet Cure), Liquid
Membrane( preferred method)
When can the curing compound be sprayed on concrete surface? - ANSWER-
immediately after film disappeared
What is the concrete paving finishing tolerance? - ANSWER-1/4" for 5' or 1/8th
for 10'
How is finishing tolerances tested - ANSWER-by means of string line or straight
edge.
String line: for alignment and grade
Straight edge: finishing
What are the testing methods of concrete? - ANSWER-Air: 5.0%, Slump: 3-4" (+/-
.5), Temp: Min 40-55 and MAx- 90 degrees
What is the air acceptance? - ANSWER-+/- 0.5 to 1.5%
What is the purpose of slump test? - ANSWER-To test workability of concrete
How long should Longitudinal joints be? - ANSWER-Should not exceed 14'