MMET 207 Exam III Questions With Correct
Answers
1000 Al - CORRECT ANSWER✔✔-commercially pure aluminum (99%
| | | | | | | |
minimum)
2000 Al - CORRECT ANSWER✔✔-copper
| | | |
3000 Al - CORRECT ANSWER✔✔-manganese
| | | |
4000 Al - CORRECT ANSWER✔✔-silicon
| | | |
5000 Al - CORRECT ANSWER✔✔-magnesium
| | | |
6000 Al - CORRECT ANSWER✔✔-magnesium and silicon
| | | | | |
7000 Al - CORRECT ANSWER✔✔-zinc
| | | |
7000-F - CORRECT ANSWER✔✔-zinc; as fabricated
| | | | |
,4000-W - CORRECT ANSWER✔✔-silicon; solution heat treated
| | | | | |
3000-O - CORRECT ANSWER✔✔-manganese; annealed
| | | |
5000-H12 - CORRECT ANSWER✔✔-magnesium; 1/4 strain hardened
| | | | | |
3000-H18 - CORRECT ANSWER✔✔-manganese; full strain harden
| | | | | |
What Aluminum series are heat treatable? - CORRECT ANSWER✔✔-
| | | | | | | |
2000, 6000, 7000
| |
What aluminum series are not heat treatable? - CORRECT ANSWER✔✔-
| | | | | | | | |
1000, 3000, 4000, 5000
| | |
2000-T3 - CORRECT ANSWER✔✔-copper; furnace solution heated,
| | | | | | |
quenched and COLD WORKED | | |
6000-T4 - CORRECT ANSWER✔✔-magnesium and silicon; furnace
| | | | | | |
solution heat treated, quenched and NATURALLY AGED
| | | | | |
7000-T6 - CORRECT ANSWER✔✔-zinc; furnace solution heat treated,
| | | | | | | |
quenched and FURNACE AGED| | |
, What are the physical properties of aluminum compared to other
| | | | | | | | | |
metals? - CORRECT ANSWER✔✔-lighter than all other engineering
| | | | | | | |
metals, high thermal and electrical conductivity, good corrosion
| | | | | | | |
resistance in atmospheric environment
| | |
Aluminum has how much of the conductivity of pure copper? -
| | | | | | | | | | |
CORRECT ANSWER✔✔-60% |
Which has a higher conductivity per unit mass, aluminum or copper? -
| | | | | | | | | | | |
CORRECT ANSWER✔✔-aluminum |
How is precipitation hardening done? - CORRECT ANSWER✔✔-
| | | | | | |
temperature raised to about 800F, water quenched and then aged
| | | | | | | | |
What does Fe do in aluminum? - CORRECT ANSWER✔✔-increases the
| | | | | | | | | |
strength and hardness and reduces hot-cracking in casting
| | | | | | |
What does Mn do in aluminum? - CORRECT ANSWER✔✔-improves
| | | | | | | | |
ductility and impact strength, castability and reduces shrinkage
| | | | | | |
What does Si do in aluminum? - CORRECT ANSWER✔✔-increases
| | | | | | | | |
fluidity and corrosion resistance, makes it difficult to machine
| | | | | | | |
Answers
1000 Al - CORRECT ANSWER✔✔-commercially pure aluminum (99%
| | | | | | | |
minimum)
2000 Al - CORRECT ANSWER✔✔-copper
| | | |
3000 Al - CORRECT ANSWER✔✔-manganese
| | | |
4000 Al - CORRECT ANSWER✔✔-silicon
| | | |
5000 Al - CORRECT ANSWER✔✔-magnesium
| | | |
6000 Al - CORRECT ANSWER✔✔-magnesium and silicon
| | | | | |
7000 Al - CORRECT ANSWER✔✔-zinc
| | | |
7000-F - CORRECT ANSWER✔✔-zinc; as fabricated
| | | | |
,4000-W - CORRECT ANSWER✔✔-silicon; solution heat treated
| | | | | |
3000-O - CORRECT ANSWER✔✔-manganese; annealed
| | | |
5000-H12 - CORRECT ANSWER✔✔-magnesium; 1/4 strain hardened
| | | | | |
3000-H18 - CORRECT ANSWER✔✔-manganese; full strain harden
| | | | | |
What Aluminum series are heat treatable? - CORRECT ANSWER✔✔-
| | | | | | | |
2000, 6000, 7000
| |
What aluminum series are not heat treatable? - CORRECT ANSWER✔✔-
| | | | | | | | |
1000, 3000, 4000, 5000
| | |
2000-T3 - CORRECT ANSWER✔✔-copper; furnace solution heated,
| | | | | | |
quenched and COLD WORKED | | |
6000-T4 - CORRECT ANSWER✔✔-magnesium and silicon; furnace
| | | | | | |
solution heat treated, quenched and NATURALLY AGED
| | | | | |
7000-T6 - CORRECT ANSWER✔✔-zinc; furnace solution heat treated,
| | | | | | | |
quenched and FURNACE AGED| | |
, What are the physical properties of aluminum compared to other
| | | | | | | | | |
metals? - CORRECT ANSWER✔✔-lighter than all other engineering
| | | | | | | |
metals, high thermal and electrical conductivity, good corrosion
| | | | | | | |
resistance in atmospheric environment
| | |
Aluminum has how much of the conductivity of pure copper? -
| | | | | | | | | | |
CORRECT ANSWER✔✔-60% |
Which has a higher conductivity per unit mass, aluminum or copper? -
| | | | | | | | | | | |
CORRECT ANSWER✔✔-aluminum |
How is precipitation hardening done? - CORRECT ANSWER✔✔-
| | | | | | |
temperature raised to about 800F, water quenched and then aged
| | | | | | | | |
What does Fe do in aluminum? - CORRECT ANSWER✔✔-increases the
| | | | | | | | | |
strength and hardness and reduces hot-cracking in casting
| | | | | | |
What does Mn do in aluminum? - CORRECT ANSWER✔✔-improves
| | | | | | | | |
ductility and impact strength, castability and reduces shrinkage
| | | | | | |
What does Si do in aluminum? - CORRECT ANSWER✔✔-increases
| | | | | | | | |
fluidity and corrosion resistance, makes it difficult to machine
| | | | | | | |