1|Page



CWB Level 2 Visual Weld Inspector Exam 2025 –
Study Guide, Requirements, and Practice Questions



Prepare for the CWB Level 2 Visual Weld Inspector Exam (Canadian Welding Bureau) with
this complete 2025 study guide. Learn exam requirements, visual inspection techniques, sample
questions, pass rates, and tips to become a certified welding inspector in Canada. Ideal for
welders, quality inspectors, and NDT professionals looking to advance their careers.




CWB Level 2 Visual Weld Inspector Exam,
CWB welding inspector certification,
CWB Level 2 exam study guide 2025,
CWB visual inspection training,



Why is it possible for some multipass welds to have higher toughness than a single pass weld - ANSWER-
The passes in the multipass weld refine the underlying grain structure



The amount of dilution of weld metal by the parent metal - ANSWER-is mostly dependent on the joint
design and welding process



Restraint is usually higher in - ANSWER-Groove welds than in fillet welds



The G-BOP test is suitable to study crack susceptibility relating to - ANSWER-Hydrogen -cracking in the
heat affected zone



What is the heat input efficiency of the SMAW process - ANSWER-50 - 85



In some steels a very slow cooling rate may procedure a - ANSWER-soft, coarse grain structure with low
toughness

,2|Page




Sometimes an unwanted microstructure can be refined and altered by reheating - ANSWER-Into
normalizing range, where it will re-crystalize and transform back into small austenite grains



Hydrogen entrapped in the solidified weld metal - ANSWER-Can not escape into the atmosphere before
it causes cracking



According to CSA W59, the SAW process can be used without preheat if adequate energy input is
ensured. This is applicable when making - ANSWER-Fillet welds in one pass



When welding alloyed structural steels the risk of cracking depends mainly on - ANSWER-chromium and
nickel content




Welding codes normally require a waiting period between welding and inspection because - ANSWER-
hydrogen induced cracks (HICC) may occur several hours after the weld has solidified



What is the main reason for pre-heating - ANSWER-to reduce the hydrogen content of the weld by
diffusion



The tekkan test is suitable to study crack susceptibility in a - ANSWER-Groove weld



Lamellar tearing is most likely to occur in which of the following - ANSWER-thick T-groove welds



During welding, the proportion of heat energy that enters the plate is referred to as its efficiency. What is
the efficiency dependent on - ANSWER-The welding process



When the alloy content of a structural steel us sufficiently high that HAZ hardness cannot be controlled -
ANSWER-The only remaining factor which can be controlled is hydrogen content



In arc welding, the area of the base metal adjacent to the fusion line which is not melted is called -
ANSWER-The Heat Affected Zone

,3|Page




Process that are not hydrogen controlled may require - ANSWER-Higher preheat temperatures for
thicker plates



What joints provide the most dilution - ANSWER-The square groove weld with zero root opening



what electrode type is often required if stress relieving operation are planned on the fabricated structure
to maintain the same yield strength and tensile strength - ANSWER-Molybdenum-bearing electrodes



The type of microstructure and susceptibility to cracking of a heat affected zone depends on - ANSWER-
Hardenability of the steel and the weld cooling rate



The level of preheat required is typically derived from the - ANSWER-plate thickness and the carbon
content of the steel



Submerged arc welding has a process efficiency of - ANSWER-90% to 99%



Covered electrodes that use basic coatings - ANSWER-Reduce electrodes that use basic coatings



The extent to which grain growth in HAZ occurs depends on - ANSWER-The energy input



For given set of welding parameters, an increase in travel speed will - ANSWER-Decrease the heat input



When weldling structural steels the main reason for preheating is - ANSWER-to allow hydrogen to escape



Crack can form in the parent material beneath the weld. This form of cracking is called - ANSWER-
Lamellar tearing



Good fracture toughness normally requires - ANSWER-A fine grain structure

, 4|Page


The solidification structure that results from a slow welding speed can be described as - ANSWER-A short
weld pool with solidifying crystals growing from the back of the pool



Beyond a certain thickness the cooling rate is independent of thickness. At about what thickness does
this occur in carbon manganese steels - ANSWER-38mm (1-1/2")



Steels can be grouped into three zones based on their carbon content and carbon equivalent. The HAZ
hardness of which group of steels can be controlled by cooling rate - ANSWER-Zone 2



In general, the higher the heat input - ANSWER-The slower the weld cooling rate



Steels can be grouped into three zones based on their carbon content and carbon equivalent. Steels in
which Zone are not prone to hydrogen cracking - ANSWER-Zone 1



Heat input from welding - ANSWER-determines the amount of component distortion during phase
transformations



Hydrogen cracking in carbon manganese steels - ANSWER-Can occur in many areas of the welds



An Arc of 300 amps and 30 volts will produce - ANSWER-9000 joules per second (300 x 30)



The peak temperature within the heat affected zone changes with distance from the fusion line. What
peak temperature is exceeded in partially transformed region - ANSWER-723



According to CSA W59, a damaged container of low alloy SMAW electrodes must be - ANSWER-re-baked
at temperatures between 230 C and 260 C



During arc welding there is a zone adjacent to the weld metal that reaches high temperatures but does
not melt. What is the name of this region - ANSWER-Heat affected zone



Not all the heat energy produced during welding will enter the plate as heat energy. What is this
phenomenon known as - ANSWER-the efficiency

Document information

Uploaded on
November 11, 2025
Number of pages
85
Written in
2025/2026
Type
Exam (elaborations)
Contains
Questions & answers
$24.99

Wrong document? Swap it for free Within 14 days of purchase and before downloading, you can choose a different document. You can simply spend the amount again.
Written by students who passed
Immediately available after payment
Read online or as PDF

Seller avatar
Reputation scores are based on the amount of documents a seller has sold for a fee and the reviews they have received for those documents. There are three levels: Bronze, Silver and Gold. The better the reputation, the more your can rely on the quality of the sellers work.
QUIZSOLUTIONS
3.0
(1)
Sold
13
Followers
5
Items
952
Last sold
11 months ago


Why students choose Stuvia

Created by fellow students, verified by reviews

Quality you can trust: written by students who passed their tests and reviewed by others who've used these notes.

Didn't get what you expected? Choose another document

No worries! You can instantly pick a different document that better fits what you're looking for.

Pay as you like, start learning right away

No subscription, no commitments. Pay the way you're used to via credit card and download your PDF document instantly.

Student with book image

“Bought, downloaded, and aced it. It really can be that simple.”

Alisha Student

Working on your references?

Create accurate citations in APA, MLA and Harvard with our free citation generator.

Working on your references?

Frequently asked questions