The major advantage of electron beam welding process is - CORRECT ANSWERS
full penetration welds on thick material in one pass
The progress of welding with Electroslag welding process is - CORRECT
ANSWERS Vertical up
Explosion welding - CORRECT ANSWERS is solid state process in which
coalescence is produced through high speed impacting of two or more
materials by controlled detonation
A typical application for thermite welding is - CORRECT ANSWERS joining of
rails
Welding without filler metal with GTAW process is referred to as - CORRECT
ANSWERS autogenous welding
A typical weld flaw associated with GTAW process is - CORRECT ANSWERS
porosity
SMAW power sources typically have a volt-ampere curve that is - CORRECT
ANSWERS drooping
Once a box of E49XX low hydrogen electrodes has been opened the electrodes
may remain at ambient temperature for up to a maximum of - CORRECT
ANSWERS 4 hours
,CWB LEVEL 2 VISUAL WELD INSPECTOR EXAM
2024 NEWEST ACTUAL EXAM COMPLETE 1000
QUESTIONS AND CORRECT DETAILED ANSWERS
(VERIFIED ANSWERS) |ALREADY GRADED A+//
BRAND NEW!!
Shielded Metal ARC Welding (SMAW) process - CORRECT ANSWERS establishes
an arc between the end of a covered electrode and the work piece.
The spray mode of metal transfer is achieved with - CORRECT ANSWERS high
amperage, high voltage and argon-rich shielding gas
digital wire feeders - CORRECT ANSWERS have feedback systems to maintain
the preset wire feed speed
wire designated by CSA standard W48 as an E491T-9MJ-H8 - CORRECT
ANSWERS Results in weld deposit with a maximum of 8 ml diffusible hydrogen
per 100 g of weld metal
A consumable electrode is: - CORRECT ANSWERS AN electrode which melts
and provides metal to fill the joint
The weld heat affected zone is: - CORRECT ANSWERS the portion of the base
metal adjacent to the weld metal whose properties have been changed due to
the heat of welding
When an arc is formed between two electrodes - CORRECT ANSWERS
electricity flows from negative cathode to positive anode
The magnetic pinch force helps in the process of the detaching the molten
metal drops from the electrode tip. The magnetic force - CORRECT ANSWERS
,CWB LEVEL 2 VISUAL WELD INSPECTOR EXAM
2024 NEWEST ACTUAL EXAM COMPLETE 1000
QUESTIONS AND CORRECT DETAILED ANSWERS
(VERIFIED ANSWERS) |ALREADY GRADED A+//
BRAND NEW!!
increases as the square of the current causing smaller and smaller droplets to
be detached
The electric current for welding must be transformed from - CORRECT
ANSWERS High voltage, low amperage to low voltage, high amperage
Self shield flux cored wires are - CORRECT ANSWERS better able to tolerate air
currents
The AWS classes metal cored wire along with - CORRECT ANSWERS solid wires
SAW Fluxes that significantly influence the composition of the weld metal
through slag/metal reactions are called - CORRECT ANSWERS active
Resistance welding of aluminum - CORRECT ANSWERS Can be done but with
greater difficulty due to its low resistivity
The plasma arc welding process is similar to what other welding process in
principles of operation - CORRECT ANSWERS GTAW
For a flat weld profile and good penetration profile using the MCAW process -
CORRECT ANSWERS 15 degree travel angle using push technique should be
used
, CWB LEVEL 2 VISUAL WELD INSPECTOR EXAM
2024 NEWEST ACTUAL EXAM COMPLETE 1000
QUESTIONS AND CORRECT DETAILED ANSWERS
(VERIFIED ANSWERS) |ALREADY GRADED A+//
BRAND NEW!!
What is the effect of tip to work distance (electrical sickout on deposition rate
of submerged are welding - CORRECT ANSWERS decreasing tip to work
distance without adjusting any other variable will cause a increase in
deposition rate
Electrode stick out is measured - CORRECT ANSWERS From tip of nozzle to end
of electrode
Contact tip-to-work is the sum (CTTW) - CORRECT ANSWERS of the electrode
extension and arc length
Increasing electrical sickout - CORRECT ANSWERS decreases voltage, decreases
current and increases resistance
Which welding process for GMAW has large weld pool and is rather large and
difficult to control out of position - CORRECT ANSWERS Spray transfer
Which welding process for GMAW has excessive spatter - CORRECT ANSWERS
Globular transfer
Which welding process for GMAW usually has lack of fusion - CORRECT
ANSWERS Short Circuit
what electrodes never go in holding or baking oven - CORRECT ANSWERS
cellulosic
2024 NEWEST ACTUAL EXAM COMPLETE 1000
QUESTIONS AND CORRECT DETAILED ANSWERS
(VERIFIED ANSWERS) |ALREADY GRADED A+//
BRAND NEW!!
The major advantage of electron beam welding process is - CORRECT ANSWERS
full penetration welds on thick material in one pass
The progress of welding with Electroslag welding process is - CORRECT
ANSWERS Vertical up
Explosion welding - CORRECT ANSWERS is solid state process in which
coalescence is produced through high speed impacting of two or more
materials by controlled detonation
A typical application for thermite welding is - CORRECT ANSWERS joining of
rails
Welding without filler metal with GTAW process is referred to as - CORRECT
ANSWERS autogenous welding
A typical weld flaw associated with GTAW process is - CORRECT ANSWERS
porosity
SMAW power sources typically have a volt-ampere curve that is - CORRECT
ANSWERS drooping
Once a box of E49XX low hydrogen electrodes has been opened the electrodes
may remain at ambient temperature for up to a maximum of - CORRECT
ANSWERS 4 hours
,CWB LEVEL 2 VISUAL WELD INSPECTOR EXAM
2024 NEWEST ACTUAL EXAM COMPLETE 1000
QUESTIONS AND CORRECT DETAILED ANSWERS
(VERIFIED ANSWERS) |ALREADY GRADED A+//
BRAND NEW!!
Shielded Metal ARC Welding (SMAW) process - CORRECT ANSWERS establishes
an arc between the end of a covered electrode and the work piece.
The spray mode of metal transfer is achieved with - CORRECT ANSWERS high
amperage, high voltage and argon-rich shielding gas
digital wire feeders - CORRECT ANSWERS have feedback systems to maintain
the preset wire feed speed
wire designated by CSA standard W48 as an E491T-9MJ-H8 - CORRECT
ANSWERS Results in weld deposit with a maximum of 8 ml diffusible hydrogen
per 100 g of weld metal
A consumable electrode is: - CORRECT ANSWERS AN electrode which melts
and provides metal to fill the joint
The weld heat affected zone is: - CORRECT ANSWERS the portion of the base
metal adjacent to the weld metal whose properties have been changed due to
the heat of welding
When an arc is formed between two electrodes - CORRECT ANSWERS
electricity flows from negative cathode to positive anode
The magnetic pinch force helps in the process of the detaching the molten
metal drops from the electrode tip. The magnetic force - CORRECT ANSWERS
,CWB LEVEL 2 VISUAL WELD INSPECTOR EXAM
2024 NEWEST ACTUAL EXAM COMPLETE 1000
QUESTIONS AND CORRECT DETAILED ANSWERS
(VERIFIED ANSWERS) |ALREADY GRADED A+//
BRAND NEW!!
increases as the square of the current causing smaller and smaller droplets to
be detached
The electric current for welding must be transformed from - CORRECT
ANSWERS High voltage, low amperage to low voltage, high amperage
Self shield flux cored wires are - CORRECT ANSWERS better able to tolerate air
currents
The AWS classes metal cored wire along with - CORRECT ANSWERS solid wires
SAW Fluxes that significantly influence the composition of the weld metal
through slag/metal reactions are called - CORRECT ANSWERS active
Resistance welding of aluminum - CORRECT ANSWERS Can be done but with
greater difficulty due to its low resistivity
The plasma arc welding process is similar to what other welding process in
principles of operation - CORRECT ANSWERS GTAW
For a flat weld profile and good penetration profile using the MCAW process -
CORRECT ANSWERS 15 degree travel angle using push technique should be
used
, CWB LEVEL 2 VISUAL WELD INSPECTOR EXAM
2024 NEWEST ACTUAL EXAM COMPLETE 1000
QUESTIONS AND CORRECT DETAILED ANSWERS
(VERIFIED ANSWERS) |ALREADY GRADED A+//
BRAND NEW!!
What is the effect of tip to work distance (electrical sickout on deposition rate
of submerged are welding - CORRECT ANSWERS decreasing tip to work
distance without adjusting any other variable will cause a increase in
deposition rate
Electrode stick out is measured - CORRECT ANSWERS From tip of nozzle to end
of electrode
Contact tip-to-work is the sum (CTTW) - CORRECT ANSWERS of the electrode
extension and arc length
Increasing electrical sickout - CORRECT ANSWERS decreases voltage, decreases
current and increases resistance
Which welding process for GMAW has large weld pool and is rather large and
difficult to control out of position - CORRECT ANSWERS Spray transfer
Which welding process for GMAW has excessive spatter - CORRECT ANSWERS
Globular transfer
Which welding process for GMAW usually has lack of fusion - CORRECT
ANSWERS Short Circuit
what electrodes never go in holding or baking oven - CORRECT ANSWERS
cellulosic