AMPP CIP Level 1 - Theory - Chapter 15 Exam |
Questions with 100% Correct Answers | Verified |
Latest Update 2026
Save
Terms in this set (23)
Impurities or contaminants on the Trash in film
surface of the substrate, seen
through the coating once it dries.
Soft and pliable coatings that can be Peeling
pulled away from the substrate
A loss of adhesion between coats Delamination
Breaks in the coating that go Cracking
completely through the coating film
to the substrate.
The formation of small bowl-shaped Cratering
depressions in the coating film
caused by trapped air are called.
What are some issues that could extreme humidity
cause non-drying film to occur? wrong curing agent added
applying the coating too thick
applying the coating at the end of its pot life
Questions with 100% Correct Answers | Verified |
Latest Update 2026
Save
Terms in this set (23)
Impurities or contaminants on the Trash in film
surface of the substrate, seen
through the coating once it dries.
Soft and pliable coatings that can be Peeling
pulled away from the substrate
A loss of adhesion between coats Delamination
Breaks in the coating that go Cracking
completely through the coating film
to the substrate.
The formation of small bowl-shaped Cratering
depressions in the coating film
caused by trapped air are called.
What are some issues that could extreme humidity
cause non-drying film to occur? wrong curing agent added
applying the coating too thick
applying the coating at the end of its pot life