AMPP CIP LEVEL 1 - Basic Coating Inspector
Theory Exam Questions and Correct
Answers
Question 1
What is the recommended maximum RH during cure time?
Correct Answer
RH should stay below 85% unless specific humidity is required for cure.
Question 2
What is ASTM D1730 Type B?
Correct Answer
Chemical Treatment.
Question 3
What is ASTM D714?
Correct Answer
Standard Test Method for Evaluating Degree of Blistering of Paints.
Question 4
What is alligatoring?
Correct Answer
Large cracks resembling alligator skin.
Page 1 of 93
,Question 5
What are the benefits of fluoropolymers?
Correct Answer
Reduced friction, increased surface resistivity and lubricity, non-stick, non-wetting,
and abrasion resistance.
Question 6
Why is thinning used?
Correct Answer
To reduce viscosity for consistent spray pattern or film.
Question 7
What are the components of dry abrasive blasting equipment?
Correct Answer
Air compressor, dryer, blast pot, operator controls, air filter, air supply hose, CO
monitor, hose, couplings, nozzle.
Question 8
What can high relative humidity (RH) cause during curing?
Correct Answer
High RH may cause solvent entrapment and/or prolong curing times.
Question 9
What is flash rusting?
Correct Answer
Rusting caused by high humidity or low surface temperatures.
Page 2 of 93
,Question 10
What is localized corrosion?
Correct Answer
Corrosion that occurs in specific areas.
Question 11
What is inorganic non-convertible thermoplastic?
Correct Answer
Coating that softens upon heating and hardens upon cooling.
Question 12
What are the probable causes of Dry Spray?
Correct Answer
Improper application technique, rapid evaporation of solvents, incorrect thinner.
Question 13
How does general corrosion affect the surface?
Correct Answer
Results in general thinning of affected surface.
Question 14
When are vinyl ester coatings used?
Correct Answer
As interior lining when storing aggressive chemicals such as acids and alkaline.
Question 15
What is the purpose of formulating multi-coat systems containing the same generic
type?
Correct Answer
To act as both a primer and topcoat
Page 3 of 93
, Question 16
What are some examples of solvents used in coatings?
Correct Answer
Acetone, toluene, xylene, and ethyl acetate.
Question 17
How is Relative Humidity calculated?
Correct Answer
(amount of water vapor/maximum amount of water vapor air can hold) x 100
Question 18
Is the coin rub test quantifiable?
Correct Answer
No, it is a subjective test without an industry standard
Question 19
What should the inspector know about thinners?
Correct Answer
Types and amounts that can be added.
Question 20
What induces the chemical reaction in the resin?
Correct Answer
Oxygen reacting with the oil.
Page 4 of 93
Theory Exam Questions and Correct
Answers
Question 1
What is the recommended maximum RH during cure time?
Correct Answer
RH should stay below 85% unless specific humidity is required for cure.
Question 2
What is ASTM D1730 Type B?
Correct Answer
Chemical Treatment.
Question 3
What is ASTM D714?
Correct Answer
Standard Test Method for Evaluating Degree of Blistering of Paints.
Question 4
What is alligatoring?
Correct Answer
Large cracks resembling alligator skin.
Page 1 of 93
,Question 5
What are the benefits of fluoropolymers?
Correct Answer
Reduced friction, increased surface resistivity and lubricity, non-stick, non-wetting,
and abrasion resistance.
Question 6
Why is thinning used?
Correct Answer
To reduce viscosity for consistent spray pattern or film.
Question 7
What are the components of dry abrasive blasting equipment?
Correct Answer
Air compressor, dryer, blast pot, operator controls, air filter, air supply hose, CO
monitor, hose, couplings, nozzle.
Question 8
What can high relative humidity (RH) cause during curing?
Correct Answer
High RH may cause solvent entrapment and/or prolong curing times.
Question 9
What is flash rusting?
Correct Answer
Rusting caused by high humidity or low surface temperatures.
Page 2 of 93
,Question 10
What is localized corrosion?
Correct Answer
Corrosion that occurs in specific areas.
Question 11
What is inorganic non-convertible thermoplastic?
Correct Answer
Coating that softens upon heating and hardens upon cooling.
Question 12
What are the probable causes of Dry Spray?
Correct Answer
Improper application technique, rapid evaporation of solvents, incorrect thinner.
Question 13
How does general corrosion affect the surface?
Correct Answer
Results in general thinning of affected surface.
Question 14
When are vinyl ester coatings used?
Correct Answer
As interior lining when storing aggressive chemicals such as acids and alkaline.
Question 15
What is the purpose of formulating multi-coat systems containing the same generic
type?
Correct Answer
To act as both a primer and topcoat
Page 3 of 93
, Question 16
What are some examples of solvents used in coatings?
Correct Answer
Acetone, toluene, xylene, and ethyl acetate.
Question 17
How is Relative Humidity calculated?
Correct Answer
(amount of water vapor/maximum amount of water vapor air can hold) x 100
Question 18
Is the coin rub test quantifiable?
Correct Answer
No, it is a subjective test without an industry standard
Question 19
What should the inspector know about thinners?
Correct Answer
Types and amounts that can be added.
Question 20
What induces the chemical reaction in the resin?
Correct Answer
Oxygen reacting with the oil.
Page 4 of 93