AMPP CIP Level 1 - Theory - Chapter 15
Exam Questions and Answers with
Verified Solutions | Latest Updated 2026
Impurities or contaminants on Trash in film
the surface of the substrate,
seen through the coating once
it dries.
Soft and pliable coatings that Peeling
can be pulled away from the
substrate
A loss of adhesion between Delamination
coats
Breaks in the coating that go Cracking
completely through the
coating film to the substrate.
The formation of small Cratering
bowl-shaped depressions in
the coating film caused by
trapped air are called.
What are some issues that extreme humidity wrong curing
could cause non-drying film to agent added applying the coating
occur? too thick applying the coating at the
end of its pot life
Exam Questions and Answers with
Verified Solutions | Latest Updated 2026
Impurities or contaminants on Trash in film
the surface of the substrate,
seen through the coating once
it dries.
Soft and pliable coatings that Peeling
can be pulled away from the
substrate
A loss of adhesion between Delamination
coats
Breaks in the coating that go Cracking
completely through the
coating film to the substrate.
The formation of small Cratering
bowl-shaped depressions in
the coating film caused by
trapped air are called.
What are some issues that extreme humidity wrong curing
could cause non-drying film to agent added applying the coating
occur? too thick applying the coating at the
end of its pot life