• Wrong document? Swap it for free
  • Written by students who passed
  • Immediately available after payment
  • Read online or as PDF
Sell
Where do you study
Your language
Document preview thumbnail
Preview 3 out of 20 pages
Exam (elaborations)

ACI Concrete Field-Testing Technician- Grade I Latest Exam 2026 Verified Correct Answers.

Document preview thumbnail
Preview 3 out of 20 pages

ACI Concrete Field-Testing Technician- Grade I Latest Exam 2026 Verified Correct Answers.

Content preview

ACI Concrete Field-Testing Technician- Grade I
Latest Exam 2026 Verified Correct Answers.



The outside diameter or side dimension of the vibrating element must be at least
_____ but not greater than _____. - CORRECT ANSWER>>0.75 in. [19 mm], 1.50 in. [38
mm]


A plastic container can be used for the measure in this method. True or False?
- CORRECT ANSWER>>False, measure must be steel or another suitable metal


What is the minimum thickness of a metal strike-off plate? - CORRECT ANSWER>>1/4
in. [6 mm]


What is the minimum thickness for a glass or acrylic strike-off plate? -
CORRECT ANSWER>>1/2 in. [12 mm]


What is the specified weight of the mallet used on measures that are 0.5
ft^3 [14 L] or smaller? - CORRECT ANSWER>>1.25 +- 0.50 lb. [600 +- 200 g]


Measures other than air meter bowls used for this test must conform to
ASTM _____. - CORRECT ANSWER>>C29

,Air meter bowls used for this test must conform to ASTM _____ and be calibrated for
volumee according to ASTM _____. - CORRECT ANSWER>>C231, C29 The concrete
sample must be obtained in accodance with what ASTM method? -

CORRECT ANSWER>>C172


What method of consolidation must be used when the slump is greater than
3 in. [75 mm]? - CORRECT ANSWER>>Rodding


What method of consolidation must be used when the slump is less than 1
in. (25 mm]? - CORRECT ANSWER>>Vibration


If rodding is the method of consolidation being used, the measure must be
filled in how many layers? - CORRECT ANSWER>>3


For a measure of 0.5 ft^3 [14 L], what is the required number of strokes of
the tamping rod for consolidation of each layer? - CORRECT ANSWER>>25


When rodding the middle and the top layers, the tamping rod should penetrate into
the layer below approximately _____. - CORRECT ANSWER>>1 in. [25 mm]


If vibration is the method of consolidation, the measure must be filled in
_____ approximately equal layers. - CORRECT ANSWER>>2

, If, after consolidation of the final layer, the concrete level is 1/2 in. (13 mm)
above the top of the measure, what should be done? -
CORRECT ANSWER>>Remove a representative portion of the excess concrete with a
trowel or scoop


After consolidation of the final layer, an excess of concrete ____ above the top of the
measure is considered optimum. - CORRECT ANSWER>>1/8 in. [3 mm]


After completing the strike-off procedure, what must be done before weighing the
measure and sample? - CORRECT ANSWER>>Clean off any excess concrete


The pressure method of determining air content can be used on concrete
containing _____ _____ aggregate. - CORRECT ANSWER>>Relatively Dense


The pressure method of determining air content cannot be used on
concrete containing the following types of aggregates, _____, _____, _____.
- CORRECT ANSWER>>Lightweight, air-cooled blast furnace slag, or
aggregates of high porosity


What is the minimum allowable capacity of the measuring bowl used in this
test method? - CORRECT ANSWER>>6 L (0.20 ft^3)


What are the required characteristics of the tamping rod used in this test method? -
CORRECT ANSWER>>Round, straight steel rod, with a 16 mm [5/8 in.] +- 2 mm [1/16
in.] diameter, length at least 100 mm [4 in.] greater than the depth of the measuring

Document information

Uploaded on
April 4, 2026
Number of pages
20
Written in
2025/2026
Type
Exam (elaborations)
Contains
Questions & answers
$12.49

Wrong document? Swap it for free Within 14 days of purchase and before downloading, you can choose a different document. You can simply spend the amount again.
Written by students who passed
Immediately available after payment
Read online or as PDF

Seller avatar
Reputation scores are based on the amount of documents a seller has sold for a fee and the reviews they have received for those documents. There are three levels: Bronze, Silver and Gold. The better the reputation, the more your can rely on the quality of the sellers work.
Sharonharry
5.0
(3)
Sold
12
Followers
0
Items
1295
Last sold
3 weeks ago



Why students choose Stuvia

Created by fellow students, verified by reviews

Quality you can trust: written by students who passed their tests and reviewed by others who've used these notes.

Didn't get what you expected? Choose another document

No worries! You can instantly pick a different document that better fits what you're looking for.

Pay as you like, start learning right away

No subscription, no commitments. Pay the way you're used to via credit card and download your PDF document instantly.

Student with book image

“Bought, downloaded, and aced it. It really can be that simple.”

Alisha Student

Working on your references?

Create accurate citations in APA, MLA and Harvard with our free citation generator.

Working on your references?

Frequently asked questions