"The impact toughness of the weld deposit required for the - CORRECT ANSWER:
"Why would 650 C be a better temperature to specify for a PWHT of a welded
martensitic stainless steel than - CORRECT ANSWER:
(Blank) are normally required to be welded together to avoid a gap that may initiate
cracks - CORRECT ANSWER: Backing bars
(Blank) are used to measure small dimensions where high precision is required -
CORRECT ANSWER: Micrometers
(Blank) is a solidification cavity that could appear as a lamination in the middle of an end
of section of a rolled plate - CORRECT ANSWER: Pipe
(f= V/λ)" - CORRECT ANSWER:
1) F = Size of source - CORRECT ANSWER:
100% CO2 is not generally used for GMAW of stainless steels - CORRECT ANSWER:
TRUE
2) Basic types - CORRECT ANSWER:
,2) Carefully clean off grease and dirt before welding - CORRECT ANSWER:
2) Compression - CORRECT ANSWER:
2) d= object to source distance - CORRECT ANSWER:
2) Dark circular or pear shaped marks - Developer splashes before immersing whole
film in developer - CORRECT ANSWER:
2) Developer is halted by immersion in stop bath - CORRECT ANSWER:
2) electrodes must be stored in dry, warm areas - CORRECT ANSWER:
2) EXXX-16 " - CORRECT ANSWER:
2) Intended service conditions - CORRECT ANSWER:
2) Radiographic contrast generally less than X-rays - CORRECT ANSWER:
2) Reducing the amount of oxygen and other impurities in the weld - CORRECT
ANSWER:
2) Rockwell - CORRECT ANSWER:
2) Root bend - CORRECT ANSWER:
2) Special safety precautions - CORRECT ANSWER:
,2) Steel - CORRECT ANSWER:
2) Suitability of a welding procedure - CORRECT ANSWER:
2) The ability to operate at lower temperatures for a given current density - CORRECT
ANSWER:
2) The wire diameter - CORRECT ANSWER:
3) Cannot be used on all materials e.g. aluminum - CORRECT ANSWER:
3) Controlling the bead shape and smoothness " - CORRECT ANSWER:
3) Dark branched lines, dark sports - Marks due to static electrical discharge " -
CORRECT ANSWER:
3) Film is immersed in fixer solution " - CORRECT ANSWER:
3) Greater arc stability and arc starting" - CORRECT ANSWER:
3) Metal cored types " - CORRECT ANSWER:
3) Shear" - CORRECT ANSWER:
3) Side bend" - CORRECT ANSWER:
3) slag is to be fully removed between passes and from the finished weld" - CORRECT
ANSWER:
, 3) Some defects not reliably detected " - CORRECT ANSWER:
3) Structure produced in the weld deposit" - CORRECT ANSWER:
3) Suitability of welding consumable" - CORRECT ANSWER:
3) t=Object to film distance" - CORRECT ANSWER:
3) The mode of metal transfer" - CORRECT ANSWER:
3) Tungsten" - CORRECT ANSWER:
3) Use stainless steel cleaning brushes " - CORRECT ANSWER:
3) Vickers" - CORRECT ANSWER:
4) Radiation emitted continuously " - CORRECT ANSWER:
550 C" - CORRECT ANSWER: To avoid temper embrittlement
A "pipe" is a solidification cavity in steel. Where would you most likely find such a defect
when inspecting a rolled plate - CORRECT ANSWER: in the middle of an end section
A 14% Cr martensitic steel hardened to 1000 C and air cooled proceduces - CORRECT
ANSWER: Martensite