Answers (100% Correct Answers)
The length of a fillet weld is the _______________________.
Ans: Overall length of the full size fillet.
The incomplete filling of the weld root is called __________________.
Ans: Inadequate penetration.
To zero out the dial caliper, you have to perform what function?
Ans: Close the jaws or contact points to no opening.
Locate the notch in the face plate and rotate it until the needle comes to zero.
Edges of members not subject to calculated stresses shall have no gouges deeper than
Ans: 1/8"
Weld crown in pipeline applications may also be referred to as:
Ans: Weld reinforcement
What is the acceptable amount of misalignment (hi-low) for pressure piping?
Ans: 0.0625" or 1/16"
What is the abbreviation for nondestructive testing?
Ans: NDT
What formula would you use to convert pounds per square inch to Megapascals?
© 2025 All rights reserved
, Ans: PSI X 0.00689 = MPa
CVN (Charpy V Notch) testing shall conform to _______________.
Ans: AWS B4.0
What is the abbreviation for complete joint penetration?
Ans: CJP
Upon visual examination, there shall be ___________________.
Ans: No evidence of cracks
For pipeline applications, any grinding or welding on a completed weld to correct an
individual defect or accumulation of defects in the weld that has been rejected by visual
or nondestructive testing is called a ___________________.
Ans: Repair
True or False: On a WPS, backing material, if used, will be documented on the document
for the FCAW, GMAW, GTAW and SMAW process?
Ans: True
If a WPS indicates it is to be used to weld Single Bevel groove welds, the Groove Angle
dimension provided on the WPS represents the ____________________?
Ans: Groove angle and Bevel angle
The number of bend tests required for a 3G plate test is ___________________?
Ans: 2
A WPS was established without Postweld Heat Treating (PWHT), the contractor now
wants to PWHT because of cracking issues. What should be done in this scenario?
Ans: Qualify a new WPS and a new PQR with PWHT