AMPP CIP1 EXAM WITH CORRECT
ACTUAL QUESTIONS AND CORRECTLY
WELL DEFINED ANSWERS LATEST
ALREADY GRADED A+
ASTM D 4417 Method B. How many measurements at each
location? - ANSWERS-10, record max values
High humidity when applying coatings means - ANSWERS-
Slow solvent evaporation
Which is faster - airless or conventional air spray? -
ANSWERS-Airless
Improper atomization may cause - ANSWERS-Uneven DFT,
dry spray, overspray
what to do to coating if high viscosity - ANSWERS-Add
thinner, heat the coating
,SSPC No. 12. How many candles/lumens? - ANSWERS-50
foot candles or 538 lumens
Minimum distance from edge with magnetic pull-off DFT
gage? - ANSWERS-1 inch
Testing procedure for water soluble ferrous salts -
ANSWERS-Potassium ferricyanide test
Chalking happens from what type of coating - ANSWERS-
Epoxy
Small bowl-shaped depressions in the coating film -
ANSWERS-cratering
Blister = - ANSWERS-Surface contamination
NACE SP0188 wand moves maximum speed of - ANSWERS-1
linear ft/sec
, ASTM D714 - ANSWERS-Standard Test Method for
Evaluating Degree of Blistering of Paints
Grounding the pump and fluid hose used in airless spray
prevents ____ - ANSWERS-Static sparking
Elements of a corrosion cell - ANSWERS-Anode, Cathode,
Metallic Pathway, Electrolyte
Allows passage of ions - ANSWERS-metallic pathway
List of materials in order of corrosion potential most to least
- ANSWERS-Galvanic series
Pitting or crevice corrosion is also called - ANSWERS-
Localized corrosion
Defects caused by incorrect application temps - ANSWERS-
Failure to cure, rapid solvent evaporation, poor film
formation
Primary components of liquid applied coating - ANSWERS-
Pigment, Vehicle
ACTUAL QUESTIONS AND CORRECTLY
WELL DEFINED ANSWERS LATEST
ALREADY GRADED A+
ASTM D 4417 Method B. How many measurements at each
location? - ANSWERS-10, record max values
High humidity when applying coatings means - ANSWERS-
Slow solvent evaporation
Which is faster - airless or conventional air spray? -
ANSWERS-Airless
Improper atomization may cause - ANSWERS-Uneven DFT,
dry spray, overspray
what to do to coating if high viscosity - ANSWERS-Add
thinner, heat the coating
,SSPC No. 12. How many candles/lumens? - ANSWERS-50
foot candles or 538 lumens
Minimum distance from edge with magnetic pull-off DFT
gage? - ANSWERS-1 inch
Testing procedure for water soluble ferrous salts -
ANSWERS-Potassium ferricyanide test
Chalking happens from what type of coating - ANSWERS-
Epoxy
Small bowl-shaped depressions in the coating film -
ANSWERS-cratering
Blister = - ANSWERS-Surface contamination
NACE SP0188 wand moves maximum speed of - ANSWERS-1
linear ft/sec
, ASTM D714 - ANSWERS-Standard Test Method for
Evaluating Degree of Blistering of Paints
Grounding the pump and fluid hose used in airless spray
prevents ____ - ANSWERS-Static sparking
Elements of a corrosion cell - ANSWERS-Anode, Cathode,
Metallic Pathway, Electrolyte
Allows passage of ions - ANSWERS-metallic pathway
List of materials in order of corrosion potential most to least
- ANSWERS-Galvanic series
Pitting or crevice corrosion is also called - ANSWERS-
Localized corrosion
Defects caused by incorrect application temps - ANSWERS-
Failure to cure, rapid solvent evaporation, poor film
formation
Primary components of liquid applied coating - ANSWERS-
Pigment, Vehicle