AMPP CIP1 Exam | Questions with 100% Correct Answers | Verified | Latest Update 2026/2027 A barrier coating interrupts the ______ of the electrochemical cell. - ANSWER Electrolyte Steel temp must be _ degrees less than the dew point to coat - ANSWER -5 Co-Reaction - ANSWER -* Cure by polymerization reactions between at least two chemical entities * Polymerization is also referred to as 'cross linking" * Eamples include: Epoxies, Polyurethanes, Polyureas, Polyaspartics, Polysiloxanes and several others Fusion Bond Epoxy (FBE) is most commonly used to coat ____ - ANSWER Pipe Coatings that require external moisture to cure - ANSWER -Single component polyurethane, solvent borne inorganic zinc Amine blush is likely to occur with which type of coating? - ANSWER -Epoxy Type of coating that cures fastest - ANSWER -Polyurea Mud cracking of an inorganic zinc-rich (IOZ) primer can be caused by - ANSWER -Applying it too heavily Primers commonly used for structural steel - ANSWER -Epoxy, Inorganic zinc, Organic Zinc Coatings that cure by polymerization are? - ANSWER -convertible Water borne latex coatings cure by a process known as? - ANSWER Coalescence UV light on a blasted surface can show - ANSWER -Oil Danger with sprayed polyurethane coating - ANSWER -Isocyanates ISO 8503 - ANSWER -surface roughness ISO SA 2-1/2 is similar to NACE _ and SP _ - ANSWER -2, 10 Alkyd coatings when applied to a highly alkaline surface will fail prematurely due to - ANSWER -Saponification SSPC Vis 1 rust with mill scale and rust... what grade? - ANSWER -Grade B ASTM D 4417 Method B. How many measurements at each location? - ANSWER -10, record max values High humidity when applying coatings means - ANSWER -Slow solvent evaporation Which is faster - airless or conventional air spray? - ANSWER -Airless Improper atomization may cause - ANSWER -Uneven DFT, dry spray, overspray what to do to coating if high viscosity - ANSWER -Add thinner, heat the coating SSPC No. 12. How many candles/lumens? - ANSWER -50 foot candles or 538 lumens Minimum distance from edge with magnetic pull-off DFT gage? - ANSWER -1 inch Testing procedure for water soluble ferrous salts - ANSWER -Potassium ferricyanide test Chalking happens from what type of coating - ANSWER -Epoxy Small bowl-shaped depressions in the coating film - ANSWER -cratering Blister = - ANSWER -Surface contamination NACE SP0188 wand moves maximum speed of - ANSWER -1 linear ft/sec ASTM D714 - ANSWER -Standard Test Method for Evaluating Degree of Blistering of Paints Grounding the pump and fluid hose used in airless spray prevents ____ - ANSWER -Static sparking Elements of a corrosion cell - ANSWER -Anode, Cathode, Metallic Pathway, Electrolyte Allows passage of ions - ANSWER -metallic pathway List of materials in order of corrosion potential most to least - ANSWER Galvanic series Pitting or crevice corrosion is also called - ANSWER -Localized corrosion Defects caused by incorrect application temps - ANSWER -Failure to cure, rapid solvent evaporation, poor film formation Primary components of liquid applied coating - ANSWER -Pigment, Vehicle Three methods by which coating provides corrosion control - ANSWER -Barrier, inhibitive, sacrificial Two non-convertible coatings - ANSWER -Chlorinated rubber, vinyl Four convertible coating curing mechanisms - ANSWER -Oxidation, co-reaction (polymerization), Hydration, Fusion Coating types that cure by polymerization - ANSWER -Epoxies, polyurethanes, polyureas, polyasparatics, polysiloxanies Induction time - ANSWER -Time between mixing and applying Oil based coatings applied over alkaline surfaces may result in: - ANSWER Saponification Power tool standards - ANSWER -St 2, St 3, SP 3, SP 11, SP 15 SP-10. _% staining - ANSWER -5

Vista previa del contenido

AMPP CIP1 Exam | Questions with 100% Correct
Answers | Verified | Latest Update 2026/2027
A barrier coating interrupts the ______ of the electrochemical cell. - ANSWER -
Electrolyte

Steel temp must be _ degrees less than the dew point to coat - ANSWER -5

Co-Reaction - ANSWER -* Cure by polymerization reactions between at least
two chemical entities
* Polymerization is also referred to as 'cross linking"
* Eamples include: Epoxies, Polyurethanes, Polyureas, Polyaspartics,
Polysiloxanes and several others

Fusion Bond Epoxy (FBE) is most commonly used to coat ____ - ANSWER -
Pipe

Coatings that require external moisture to cure - ANSWER -Single component
polyurethane, solvent borne inorganic zinc

Amine blush is likely to occur with which type of coating? - ANSWER -Epoxy

Type of coating that cures fastest - ANSWER -Polyurea

Mud cracking of an inorganic zinc-rich (IOZ) primer can be caused by -
ANSWER -Applying it too heavily

Primers commonly used for structural steel - ANSWER -Epoxy, Inorganic zinc,
Organic Zinc

Coatings that cure by polymerization are? - ANSWER -convertible

Water borne latex coatings cure by a process known as? - ANSWER -
Coalescence

UV light on a blasted surface can show - ANSWER -Oil

Danger with sprayed polyurethane coating - ANSWER -Isocyanates

, ISO 8503 - ANSWER -surface roughness

ISO SA 2-1/2 is similar to NACE _ and SP _ - ANSWER -2, 10

Alkyd coatings when applied to a highly alkaline surface will fail prematurely due
to - ANSWER -Saponification

SSPC Vis 1 rust with mill scale and rust... what grade? - ANSWER -Grade B

ASTM D 4417 Method B. How many measurements at each location? -
ANSWER -10, record max values

High humidity when applying coatings means - ANSWER -Slow solvent
evaporation

Which is faster - airless or conventional air spray? - ANSWER -Airless

Improper atomization may cause - ANSWER -Uneven DFT, dry spray, overspray

what to do to coating if high viscosity - ANSWER -Add thinner, heat the coating

SSPC No. 12. How many candles/lumens? - ANSWER -50 foot candles or 538
lumens

Minimum distance from edge with magnetic pull-off DFT gage? - ANSWER -1
inch

Testing procedure for water soluble ferrous salts - ANSWER -Potassium
ferricyanide test

Chalking happens from what type of coating - ANSWER -Epoxy

Small bowl-shaped depressions in the coating film - ANSWER -cratering

Blister = - ANSWER -Surface contamination

NACE SP0188 wand moves maximum speed of - ANSWER -1 linear ft/sec

Información del documento

Subido en
28 de julio de 2026
Número de páginas
9
Escrito en
2025/2026
Tipo
Examen
Contiene
Preguntas y respuestas
$12.99

¿Documento equivocado? Cámbialo gratis Dentro de los 14 días posteriores a la compra y antes de descargarlo, puedes elegir otro documento. Puedes gastar el importe de nuevo.
Escrito por estudiantes que aprobaron
Inmediatamente disponible después del pago
Leer en línea o como PDF

Seller avatar
Los indicadores de reputación están sujetos a la cantidad de artículos vendidos por una tarifa y las reseñas que ha recibido por esos documentos. Hay tres niveles: Bronce, Plata y Oro. Cuanto mayor reputación, más podrás confiar en la calidad del trabajo del vendedor.
TheExamMaestro
3.6
(18)
Vendido
149
Seguidores
5
Artículos
3668
Última venta
14 horas hace


Por qué los estudiantes eligen Stuvia

Creado por compañeros estudiantes, verificado por reseñas

Calidad en la que puedes confiar: escrito por estudiantes que aprobaron y evaluado por otros que han usado estos resúmenes.

¿No estás satisfecho? Elige otro documento

¡No te preocupes! Puedes elegir directamente otro documento que se ajuste mejor a lo que buscas.

Paga como quieras, empieza a estudiar al instante

Sin suscripción, sin compromisos. Paga como estés acostumbrado con tarjeta de crédito y descarga tu documento PDF inmediatamente.

Student with book image

“Comprado, descargado y aprobado. Así de fácil puede ser.”

Alisha Student

Preguntas frecuentes