8001. Laminated wood spars may be substituted fore solid rectangular wood spars
- Correct answer-if the same quality wood is used in both.
8002. The strength of a well-designed and properly prepared wood splice joint is
provided by the - Correct answer-glue
8003. Where is information found concerning acceptable species substitutions for
wood materials used in aircraft repair? - Correct answer-AC 43.13-1B
8004. In cases of elongated bolt holes in a wood spare or cracks in the vicinity of
bolt holes - Correct answer-a new section of spar should be spliced in or the spar
replaced entirely
8005. A faint line running across the grain of a wood spar generally indicates -
Correct answer-compression failure
8005-1. Any wooden member that has been overstressed is subject to which type of
failure? - Correct answer-compression failure
©COPYRIGHT 2025, ALL RIGHTS RESERVED 1
Questions and Answers Graded A+
8001. Laminated wood spars may be substituted fore solid rectangular wood spars
- Correct answer-if the same quality wood is used in both.
8002. The strength of a well-designed and properly prepared wood splice joint is
provided by the - Correct answer-glue
8003. Where is information found concerning acceptable species substitutions for
wood materials used in aircraft repair? - Correct answer-AC 43.13-1B
8004. In cases of elongated bolt holes in a wood spare or cracks in the vicinity of
bolt holes - Correct answer-a new section of spar should be spliced in or the spar
replaced entirely
8005. A faint line running across the grain of a wood spar generally indicates -
Correct answer-compression failure
8005-1. Any wooden member that has been overstressed is subject to which type of
failure? - Correct answer-compression failure