Answers 100% Pass
What is the distance a counterborne extends axially into a pipe? - ✔✔Counterborne
Depth
When shall incomplete fusion (IF) be considered a defect? - ✔✔If the aggregate length
of indications of IF exceeds 8% of the weld length in any weld less than 12 inches in
length.
What is another name for weld spacing? - ✔✔Pitch
The bend criteria for a Procedure Qualification Test should not have a edge radius more
than? - ✔✔1/8th inch
what is the abbreviation for cubic feet per hour? - ✔✔CFH
when qualifying a welder to make the weld on plate that is 1 inch thick what is the
minimum thickness that can be used in the test - ✔✔1/2 inch
what is the abbreviation for width of Bend specimen? - ✔✔W
what is the abbreviation for non-destructive examination - ✔✔NDE
Brittie Donald, All Rights Reserved © 2025 1
, the pqr shall list _________ values of the variables used - ✔✔actual
the standard dimensional tolerances in this specification do not apply - ✔✔To the
dimensions for test specimens.
To Annex IV.
To discontinuity acceptance limits.
A Groove melted or any reduction of the parent material adjacent to the toe or root of
the weld unfilled by weld metal is called _____________. - ✔✔undercutting
the response or evidence from the application of a non-destructive examination is called
an ______________. - ✔✔indication
In pipeline the completed weld shall ___________. - ✔✔have all spatter removed
a welder qualified on any material from M7 material is qualified the weld on what
material - ✔✔M-1 thru M-11
what is the conversion step to change PSI to KSI? - ✔✔take 3 decimal places off the PSI
value or divide PSI by 1000
True or false: for the welding of Base Metals with different M numbers a procedure
qualification test shall be made for each combination of M numbers to be joined -
✔✔True. Except that a procedure qualification test with 1 M number shall also qualify
Brittie Donald, All Rights Reserved © 2025 2