WELD INSPECTOR LEVEL 1 FINAL EXAM WITH VERIFIED QUESTIONS AND ANSWERS || ALREADY GRADED A+|| GUARANTEED PASS | LATEST VERSION 2025

Puntuación
-
Vendido
-
Páginas
61
Grado
A+
Subido en
12-07-2025
Escrito en
2024/2025

WELD INSPECTOR LEVEL 1 FINAL EXAM WITH VERIFIED QUESTIONS AND ANSWERS || ALREADY GRADED A+|| GUARANTEED PASS | LATEST VERSION 2025 In AWS D1.1 , procedures for which one of the following processes cannot be approved unless testing is carried out ? ( a ) FCAW ( b ) GMAW - S ( c ) SAW ( d ) SMAW - ANSWER-( b ) GMAW - S Which one of the following sections from the ASME Boiler and Pressure Vessel Code covers Nonferrous Material Specifications? ( a ) Section I ( b ) Section II , Part B ( c ) Section II , Part D ( d ) Section VIII , Division 2 - ANSWER-( b ) Section II , Part B True or False? The FCC structure is more closely packed than the BCC structure. ( a ) True ( b ) False - ANSWER-( a ) True The extent to which a steel forms martensite at a given cooling rate is called: ( a ) carburizing . ( b ) sensitivity . ( c ) hardenability . ( d ) temperability . - ANSWER-( c ) hardenability . True or False? Normalizing of steel involves heating into the fully austenite region followed by furnace cooling. ( a ) True ( b ) False - ANSWER-( b ) False Hot rolling is carried out: ( a ) below the lower transformation temperature . ( b ) between 723 ° C and 912 ° C . ( c ) in the austenite / ferrite region . ( d ) in the fully austenitic region . - ANSWER-( d ) in the fully austenitic region . Tempering martensite involves reheating to a temperature: ( a ) in the austenite / ferrite region . ( b ) in the fully austenitic region . ( c ) above the lower transformation temperature of 723 ° C . ( d ) below the lower transformation temperature of 723 ° C . - ANSWER-( d ) below the lower transformation temperature of 723 ° C . According to CSA Standard W59 , at what distance from the weld must the minimum preheat be maintained in 44 mm thick plate ? ( a ) 44 mm ( b ) 50 mm ( c ) 75 mm ( d ) 88 mm - ANSWER-( c ) 75 mm Visual inspection of inaccessible areas may be carried out with the use of : ( a ) gauges . ( b ) magnifying glasses . ( c ) lasers . ( d ) boroscopes . - ANSWER-( d ) boroscopes .

Mostrar más Leer menos
Institución
WELD INSPECTOR LEVEL 1
Grado
WELD INSPECTOR LEVEL 1











Ups! No podemos cargar tu documento ahora. Inténtalo de nuevo o contacta con soporte.

Escuela, estudio y materia

Institución
WELD INSPECTOR LEVEL 1
Grado
WELD INSPECTOR LEVEL 1

Información del documento

Subido en
12 de julio de 2025
Número de páginas
61
Escrito en
2024/2025
Tipo
Examen
Contiene
Preguntas y respuestas

Temas

Vista previa del contenido

WELD INSPECTOR LEVEL 1 FINAL EXAM
WITH VERIFIED QUESTIONS AND ANSWERS ||
ALREADY GRADED A+|| GUARANTEED PASS |
LATEST VERSION 2025




In AWS D1.1 , procedures for which one of the following processes cannot be
approved unless testing is carried out ?
( a ) FCAW
( b ) GMAW - S
( c ) SAW
( d ) SMAW - ANSWER-( b ) GMAW - S


Which one of the following sections from the ASME Boiler and Pressure Vessel
Code covers Nonferrous Material Specifications?
( a ) Section I
( b ) Section II , Part B
( c ) Section II , Part D
( d ) Section VIII , Division 2 - ANSWER-( b ) Section II , Part B
True or False? The FCC structure is more closely packed than the BCC
structure.
( a ) True
( b ) False - ANSWER-( a ) True


The extent to which a steel forms martensite at a given cooling rate is called:
( a ) carburizing .
( b ) sensitivity .

,( c ) hardenability .
( d ) temperability . - ANSWER-( c ) hardenability .


True or False? Normalizing of steel involves heating into the fully austenite
region followed by furnace cooling.
( a ) True
( b ) False - ANSWER-( b ) False


Hot rolling is carried out:
( a ) below the lower transformation temperature .
( b ) between 723 ° C and 912 ° C .
( c ) in the austenite / ferrite region .
( d ) in the fully austenitic region . - ANSWER-( d ) in the fully austenitic region
.


Tempering martensite involves reheating to a temperature:
( a ) in the austenite / ferrite region .
( b ) in the fully austenitic region .
( c ) above the lower transformation temperature of 723 ° C .
( d ) below the lower transformation temperature of 723 ° C . - ANSWER-( d )
below the lower transformation temperature of 723 ° C .


According to CSA Standard W59 , at what distance from the weld must the
minimum preheat be maintained in 44 mm thick plate ?
( a ) 44 mm
( b ) 50 mm
( c ) 75 mm
( d ) 88 mm - ANSWER-( c ) 75 mm

,Visual inspection of inaccessible areas may be carried out with the use of :
( a ) gauges .
( b ) magnifying glasses .
( c ) lasers .
( d ) boroscopes . - ANSWER-( d ) boroscopes .


CSA W59 states surfaces and edges that are to be welded must be free of slag ,
rust , paint and so forth within _________________ of the weld to prevent weld
contamination . ( a ) 25 mm
( b ) 50 mm
( c ) 2 x material thickness
( d ) 4 x material thickness - ANSWER-( b ) 50 mm


There is a cost to poor fit - up since a gap of _________mm or greater in a fillet
weld requires the size of fillet weld to be increased by the amount of the gap . (
a ) 1 ( b ) 1.5 ( c ) 2 ( d ) 4 - ANSWER-( c ) 2


________________ are normally required to be welded together to avoid a gap
that may initiate cracks .
( a ) Run off plates
( b ) Joint restraint bars .
( c ) Strongbacks
( d ) Backing bars - ANSWER-( d ) Backing bars


15. Which dimension should be measured when visually inspecting a
concave fillet weld ?
( a ) The smallest leg size
( b ) The penetration
( c ) The throat
( d ) The concavity - ANSWER-( c ) The throat

, For fillet welds with unequal leg sizes , where an equal leg fillet was specified ,
always measure the :
( a ) longer leg length .
( b ) shorter leg length .
( c ) throat .
( d ) face width . - ANSWER-( b ) shorter leg length .


True or False ? There is a simple relation between face width and throat size for
flare welds that can be used in all cases .
( a ) True
( b ) False - ANSWER-( b ) False


When up to 0.8 % carbon is added to iron, the resulting steel under equilibrium
conditions will have a structure of:
( a ) austenite and ferrite .
( b ) ferrite and pearlite .
( c ) ferrite and cementite .
( d ) cementite and pearlite - ANSWER-( b ) ferrite and pearlite .


A hypoeutectoid steel has:
( a ) 0.5 % carbon .
( b ) Less than 0.8 % carbon .
( c ) 0.8 % carbon .
( d ) 1.7 % carbon . - ANSWER-( b ) Less than 0.8 % carbon .


Which of the following standards / codes covers the "Design of Steel
Structures”?:
( a ) CAN / CSA S16
$22.99
Accede al documento completo:

100% de satisfacción garantizada
Inmediatamente disponible después del pago
Tanto en línea como en PDF
No estas atado a nada

Conoce al vendedor
Seller avatar
martinmwambingu54
4.0
(1)

Conoce al vendedor

Seller avatar
martinmwambingu54 Johns Hopkins University
Ver perfil
Seguir Necesitas iniciar sesión para seguir a otros usuarios o asignaturas
Vendido
7
Miembro desde
6 meses
Número de seguidores
1
Documentos
878
Última venta
1 mes hace
A+ EXAM ARCHIVES YOUR BLUEPRINT FOR ACADEMIC SUCCESS!

Welcome to A+ EXAM ARCHIVES – Your New Frontier for Academic Success on Stuvia! We\'re pioneering a fresh approach to study resources. We\'re dedicated to bringing you meticulously engineered, verified study solutions designed to unlock your full potential and drive remarkable academic success. Our commitment is clear: to provide cutting-edge content that is not only exceptionally clear and accurate but also strategically optimized to streamline your learning process. Whether you\'re aiming to master complex concepts, prepare for upcoming challenges, or simply seeking intelligent, reliable study tools, our curated collection of next-gen notes, agile summaries, and comprehensive learning frameworks is built to give you a distinct advantage. We understand that today\'s students need more than just information – they need effective, innovative solutions. That\'s why every document we create is thoughtfully developed to meet your specific learning requirements, ensuring you have the powerful tools to navigate your academic journey with absolute confidence. Join us at the forefront of smarter studying. Explore our store today and be among the first to experience a new level of academic support. Activate your A+ potential now!

Lee mas Leer menos
4.0

1 reseñas

5
0
4
1
3
0
2
0
1
0

Recientemente visto por ti

Por qué los estudiantes eligen Stuvia

Creado por compañeros estudiantes, verificado por reseñas

Calidad en la que puedes confiar: escrito por estudiantes que aprobaron y evaluado por otros que han usado estos resúmenes.

¿No estás satisfecho? Elige otro documento

¡No te preocupes! Puedes elegir directamente otro documento que se ajuste mejor a lo que buscas.

Paga como quieras, empieza a estudiar al instante

Sin suscripción, sin compromisos. Paga como estés acostumbrado con tarjeta de crédito y descarga tu documento PDF inmediatamente.

Student with book image

“Comprado, descargado y aprobado. Así de fácil puede ser.”

Alisha Student

Preguntas frecuentes