CWB Level II Key review points from Modules 1 through 22 What is the term used to describe the following condition of lost corrosion resistance? "When certain stainless steels are heated between 500-850° C, carbides form at the grain boundaries and
CWB Level II Key review points from Modules 1 through 22 What is the term used to describe the following condition of lost corrosion resistance? "When certain stainless steels are heated between 500-850° C, carbides form at the grain boundaries and cause a local depletion of chromium."